Polylactic acid (PLA) is a biodegradable polymer derived from renewable feedstocks, offering significant environmental advantages for applications in packaging, biomedical devices, and textiles. Despite its many advantages, PLA synthesis often involves energy-intensive processes that limit its sustainability. Here, we present a rapid, solvent-free preparation method for PLA synthesis employing infrared (IR) irradiation as an alternative energy source, combined with Brønsted and Lewis acid catalysts to achieve direct, stereo-controlled polymerization of lactic acid (water solution 85%) under atmosferic pressure. Through systematic evaluation of organic, inorganic, and organometallic catalysts, we identify Sc(TfO)₃, and PTSA as optimal catalysts, yielding PLA with molecular weights (Mn) until 8 kDa, within six hours at atmospheric pressure. Scaling the reaction from 2,4, 5 to 50 g demonstrated process robustness. The whole synthesis requires only 1.5 kW of energy in 6h, generates no chemical waste, and minimizes environmental impact, highlighting a sustainable, scalable approach to PLA production. This work establishes an effective balance between catalytic efficiency, polymer quality, and sustainability, offering a promising route towards greener biopolymer manufacturing aligned with global environmental goals.

Solvent-free infrared polymerization of lactic acid: toward greener PLA production

Maria Montrone;Jennifer Gubitosa;Pietro Cotugno;Gianluca Maria Farinola;Maria Annunziata M. Capozzi
2026-01-01

Abstract

Polylactic acid (PLA) is a biodegradable polymer derived from renewable feedstocks, offering significant environmental advantages for applications in packaging, biomedical devices, and textiles. Despite its many advantages, PLA synthesis often involves energy-intensive processes that limit its sustainability. Here, we present a rapid, solvent-free preparation method for PLA synthesis employing infrared (IR) irradiation as an alternative energy source, combined with Brønsted and Lewis acid catalysts to achieve direct, stereo-controlled polymerization of lactic acid (water solution 85%) under atmosferic pressure. Through systematic evaluation of organic, inorganic, and organometallic catalysts, we identify Sc(TfO)₃, and PTSA as optimal catalysts, yielding PLA with molecular weights (Mn) until 8 kDa, within six hours at atmospheric pressure. Scaling the reaction from 2,4, 5 to 50 g demonstrated process robustness. The whole synthesis requires only 1.5 kW of energy in 6h, generates no chemical waste, and minimizes environmental impact, highlighting a sustainable, scalable approach to PLA production. This work establishes an effective balance between catalytic efficiency, polymer quality, and sustainability, offering a promising route towards greener biopolymer manufacturing aligned with global environmental goals.
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11586/569680
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact